Your Position:News>Industry News
Company News Industry News

Spraying method of wine bottle of glass bottle manufacturer

Time:2020-06-09 Click:2921

The spray production line of glass wine bottle generally consists of spray room, suspension chain and oven. The glass bottle also has the front water treatment. The special attention of the glass bottle is the sewage discharge. As for the spraying quality of glass bottle, it is related to water treatment, surface cleaning of workpiece, conductivity of hook, air volume, powder spraying and operator's level.

The following methods are recommended for Trial Implementation

1. Pretreatment (CH ǔ L ǐ) segment. The pretreatment section for spraying glass wine bottles includes pre stripping, main stripping and surface adjustment. If it is in the north, the temperature of the main stripping part cannot be too low, so it needs to be kept warm. Otherwise, the treatment effect is not ideal;

2. Preheating section. After the pretreatment (CH ǔ L ǐ), it is necessary to enter the preheating section, which generally takes 8-10 minutes. When the glass bottle arrives at the powder spraying room, it is necessary to make the workpiece to be sprayed have a certain amount of waste heat, so as to increase the adhesion of the powder foam;

3. Glass bottle soot blowing purification section. If the technological requirements of the sprayed workpiece are relatively high, this section is necessary. Otherwise, if there is a lot of dust adsorbed on the workpiece, there will be a lot of particles on the surface of the processed workpiece, which will reduce the quality;

4. Powder spraying section. Glass bottle is the traditional beverage packaging container in China, and glass is also a kind of packaging material with a long history. In the case of many kinds of packaging materials pouring into the market, glass container still occupies an important position in beverage packaging, which is inseparable from its packaging characteristics which can not be replaced by other packaging materials. The key point of this paragraph is the technical problem of the duster. If you want to create a good character, it is worthwhile to pay for a skilled master.

5. Drying section. What should be noted in this section is the temperature and baking time. Generally, 180-200 ℃ is the best temperature for the powder, which depends on the material of the workpiece. There is also drying furnace from the powder room should not be too far, generally 6 meters is good.